Fracture Toughness of Samarium Cobalt Magnets

[+] Author Affiliations
Paul R. Curtin, Patricia Iglesias Victoria

Rochester Institute of Technology, Rochester, NY

Steve Constantinides

Arnold Magnetics, Rochester, NY

Paper No. IMECE2015-53435, pp. V014T11A021; 5 pages
doi:10.1115/IMECE2015-53435
From:
  • ASME 2015 International Mechanical Engineering Congress and Exposition
  • Volume 14: Emerging Technologies; Safety Engineering and Risk Analysis; Materials: Genetics to Structures
  • Houston, Texas, USA, November 13–19, 2015
  • Conference Sponsors: ASME
  • ISBN: 978-0-7918-5757-1
  • Copyright © 2015 by ASME

abstract

Samarium Cobalt (SmCo) magnets have been the magnet of choice for a variety of industries for many years due to their favorable magnetic properties. Their high coercivity, combined with a low temperature coefficient, make them the ideal permanent magnet for demanding high temperature applications. One of the biggest concerns with rare earth magnets is their brittleness. Samarium Cobalt magnets in particular are prone to fracturing during machining and assembly. In manufacturing, great care must be taken to avoid chipping or fracturing these magnets due to their brittle nature.

There are two main grades of Samarium Cobalt magnets, 1:5 and 2:17. These ratios define the nominal ratio of rare earth to transition metal content.

In this paper, an investigation is performed on the fracture toughness of permanent magnets based on the Samarium Cobalt 2:17 composition. Various techniques are used to characterize the microstructure of the material, and quantify the material properties.

Optical microscopy is used to characterize the grain structure of the material and quantify the porosity of the material after sintering. By comparing the average grain size and fracture toughness of several samples, grain size was shown to not affect fracture toughness in standard material. Latent cracks in defective material showed no preference to follow grain boundaries, oxides inclusions or voids.

River marks in fracture surfaces are seen through scanning electron microscopy, confirming the transgranular cracking pattern seen by Li et al [1]This suggests that the toughness of the material is an inherent property of the main phase, not of grain boundaries or contaminants.

Samarium Cobalt magnets exhibit both mechanical and magnetic anisotropy due to the alignment of their crystal structure in the manufacturing process.

Using Palmqvist indentation crack techniques, the magnetic orientation of the grains was seen to greatly influence the direction of crack propagation from the tip of the indenter. Measurements of fracture toughness using this technique produce highly scattered data due to this anisotropic nature of the material. Specimens loaded with the indenter axis parallel to the direction of orientation show normal Palmqvist cracks, while specimens loaded perpendicular to the direction of magnetization exhibit crack propagation initiating from the faces of the indenter.

To better quantify the material’s brittleness, fracture testing is performed on specially prepared samples to obtain an absolute measure of fracture toughness (K1c). Results show that SmCo is measurably weaker than other magnetic materials such as neodymium iron boron magnets[2]. Furthermore, neither relative concentration of Samarium nor source of raw material show notable effect on the fracture toughness of the material.

Copyright © 2015 by ASME

Figures

Tables

Interactive Graphics

Video

Country-Specific Mortality and Growth Failure in Infancy and Yound Children and Association With Material Stature

Use interactive graphics and maps to view and sort country-specific infant and early dhildhood mortality and growth failure data and their association with maternal

NOTE:
Citing articles are presented as examples only. In non-demo SCM6 implementation, integration with CrossRef’s "Cited By" API will populate this tab (http://www.crossref.org/citedby.html).

Some tools below are only available to our subscribers or users with an online account.

Related Content

Customize your page view by dragging and repositioning the boxes below.

Related eBook Content
Topic Collections

Sorry! You do not have access to this content. For assistance or to subscribe, please contact us:

  • TELEPHONE: 1-800-843-2763 (Toll-free in the USA)
  • EMAIL: asmedigitalcollection@asme.org
Sign In