Studies on Hydrogen Permeation of Weldments for Two Low-Alloyed Steels With Different Microstructures

[+] Author Affiliations
Jian Qun Tang, Jian Ming Gong

Nanjing University of Technology, Nanjing, Jiangsu, China

Paper No. PVP2011-57419, pp. 835-839; 5 pages
doi:10.1115/PVP2011-57419
From:
  • ASME 2011 Pressure Vessels and Piping Conference
  • Volume 6: Materials and Fabrication, Parts A and B
  • Baltimore, Maryland, USA, July 17–21, 2011
  • Conference Sponsors: Pressure Vessels and Piping Division
  • ISBN: 978-0-7918-4456-4
  • Copyright © 2011 by ASME

abstract

16MnR and SPV50Q low-alloyed steels, which have ferrite-pearlite and tempered martensite microstructures, respectively, are widely used to fabricate storage tanks for liquefied petroleum gas. However, during the process of operation, some cracks often occur on tanks made by these steels due to the presence of hydrogen, especially on weldments. The occurrence of this cracking is closely related to the diffusion and permeation of hydrogen in the steels. In order to explore the effect of different microstructures on hydrogen permeation and compare the hydrogen permeability of these two weldments, measurements were conducted on various metals (base metal-BM, heat-affected zone-HAZ, and welded metal-WM) cut from 16MnR and SPV50Q weldments by using electrochemical permeation tests. The results show that the microstructure has an important effect on hydrogen permeability. For 16MnR steel weldment, the diffusion coefficient of BM is the minimum due to the presence of the strong hydrogen traps in the interface between banded pearlite and matrix as well as the interface between inclusion and matrix. The microstructure of WM provides great grain boundary area as a hydrogen diffusion path and makes hydrogen easily diffuse, which results in the maximum permeation rate and diffusion coefficient. The fine-grained microstructure of normalized zone in HAZ acts as barriers for the hydrogen diffusion, which makes the permeation rate and diffusion coefficient of HAZ located between those of BM and WM. Similarly, for SPV50Q weldment, the permeation rate and diffusion coefficient increase in the order of BM, HAZ and WM. Those of BM are the minimum, which is correlated with the strong hydrogen trap due to the large quantities of dislocation within the lath martensite. Those of WM are the maximum for its strongly hydrogen diffusion path like WM of 16MnR weldment. As comparing the hydrogen permeability of 16MnR and SPV50Q weldment, the corresponding metals of the former always have greater permeation rate and diffusion coefficient than those of the latter, which is also due to its intrinsic microstructures.

Copyright © 2011 by ASME
Topics: Steel , Hydrogen

Figures

Tables

Interactive Graphics

Video

Country-Specific Mortality and Growth Failure in Infancy and Yound Children and Association With Material Stature

Use interactive graphics and maps to view and sort country-specific infant and early dhildhood mortality and growth failure data and their association with maternal

NOTE:
Citing articles are presented as examples only. In non-demo SCM6 implementation, integration with CrossRef’s "Cited By" API will populate this tab (http://www.crossref.org/citedby.html).

Some tools below are only available to our subscribers or users with an online account.

Related Content

Customize your page view by dragging and repositioning the boxes below.

Related eBook Content
Topic Collections

Sorry! You do not have access to this content. For assistance or to subscribe, please contact us:

  • TELEPHONE: 1-800-843-2763 (Toll-free in the USA)
  • EMAIL: asmedigitalcollection@asme.org
Sign In