Mechanic, Metalurgic and Factografic Characterization of a Composite of Microalloyed Steel (API X65) Cladded With Austenitic Stainless Steel (AISI 308L)

[+] Author Affiliations
Carlos R. da Cunha, Telmo R. Strohaecker

Federal University of Rio Grande do Sul

Paper No. IPC2006-10591, pp. 627-634; 8 pages
doi:10.1115/IPC2006-10591
From:
  • 2006 International Pipeline Conference
  • Volume 3: Materials and Joining; Pipeline Automation and Measurement; Risk and Reliability, Parts A and B
  • Calgary, Alberta, Canada, September 25–29, 2006
  • Conference Sponsors: Pipeline Division
  • ISBN: 0-7918-4263-0
  • Copyright © 2006 by ASME

abstract

In some offshore structures, pipes with good mechanical resistance and internal surfaces that have also good corrosion resistance are necessary. To associate these properties, one possibility is to make a cladding process in the pipe. To evaluate this kind of composite, a pipe (API X65) was clad with stainless steel (ASTM 308L) by GMAW process and sectioned in several specimens for different analyses. The work starts qualifying the quality of the composite with bending tests. The load that was recorded in this test was the guide to three-point-fatigue tests that gave us the possibility to plot an S-N curve. The tension was the most tensioned point in the specimen. To verify the metallographic conditions of both materials and the interface, metallographic analyses with a transversal cut in the specimens and hardness test across the composite were accomplished. The fatigue tested specimens were submitted to fracture analyses to know how the failure occurs. These analyses contain photos of the specimen’s fracture - showing the origin of the failure, a metallographic of the specimen’s interface to check undesired microstructures that could cause a failure and micrographs of the most tensioned point of the specimen to check the initial failure mechanism. The results in the following work show a good way of cladding process.

Copyright © 2006 by ASME

Figures

Tables

Interactive Graphics

Video

Country-Specific Mortality and Growth Failure in Infancy and Yound Children and Association With Material Stature

Use interactive graphics and maps to view and sort country-specific infant and early dhildhood mortality and growth failure data and their association with maternal

NOTE:
Citing articles are presented as examples only. In non-demo SCM6 implementation, integration with CrossRef’s "Cited By" API will populate this tab (http://www.crossref.org/citedby.html).

Some tools below are only available to our subscribers or users with an online account.

Related Content

Customize your page view by dragging and repositioning the boxes below.

Related eBook Content
Topic Collections

Sorry! You do not have access to this content. For assistance or to subscribe, please contact us:

  • TELEPHONE: 1-800-843-2763 (Toll-free in the USA)
  • EMAIL: asmedigitalcollection@asme.org
Sign In